Keep up to dateBath material | |||
Ìý | Capital cost £/bath | Net present value £/bath | Service life Years |
Enamelled cast-iron | |||
Porcelain enamelled cast-iron to BS 1189 | 420 | 468 | 60 |
Enamelled steel | |||
Vitreous enamelled pressed steel to BS 1390, steel minimum 2.2 mm thick | 375 | 554 | 35 |
Vitreous enamelled pressed steel to BS 1390, steel minimum 1.6 mm thick | 325 | 514 | 30 |
Acrylic | |||
Reinforced acrylic bath and cradle, minimum 8 mm thick, made with acrylic material tested to BS 7015 (EN 263) and constructed to meet the performance requirements of BS 4305- 1: 1989 (EN 198). | 515 | 758 | 30 |
Reinforced acrylic bath and cradle, minimum 5 mm thick, made with acrylic material tested to BS 7015 (EN 263) and constructed to meet the performance requirements of BS 4305- 1: 1989 (EN 198). | 465 | 831 | 25 |
Reinforced acrylic bath and cradle, minimum 2.7 mm thick, made with acrylic material tested to BS 7015 (EN 263) and constructed to meet the performance requirements of BS 4305- 1: 1989 (EN 198). | 375 | 928 | 15 |